Process description

The polymer melt is provided by an extruder (4) and is transported into the impregnation/calibration module (3) by a diverter valve. The belt draw-off (7) draws the rovings or strands through the entire system, through all machine modules, at constant speed.

First, the rovings are unwound in a controlled way from the unwinding creel and pass through a preheating and spreading module (2) before they reach the impregnation/calibration module (3). Here the flat, spread rovings meet the polymer melts in which the individual fibres are saturated or impregnated.

At the outlet of the impregnation/calibration module, the fibres are formed into a strand and calibrated to the required fibre content (3). The forming roller or forming roller module (5) post-forms the strands as well as smoothing and cooling them. An optional strand cooling trough (6) can supplement the system as a post-cooling section. Then the strand pelletizer (8) cuts the strands to the required pellet length.

to the product

Contact us

Our complete contact page incl. all our representations abroad can be found here:

Contact ips Agencies

ips
Intelligent Pelletizing Solutions GmbH & Co KG

Depotstraße 3, 63843 Niedernberg, Germany

By using our contact form you agree to our data protection regulations.

To combat spam requests, we use Google ReCaptcha technology, for example.

By using our contact form, your IP address will be transmitted to Google.